In the past I've see a type of aluminum alloy solder for repairing pot metal emblems, and bezels, but cannot locate a vendor. I have several of the hood scripts for "B" models that are broken and would like to repair them, as opposed to replacement.

Any help or direction is appreciated.

Rob

Dog.jpg.487f03da076af0150d2376dbd16843ed.jpgPlodding along with no job nor practical application for my existence, but still trying to fix what's broke.

 

 

Link to comment
Share on other sites

http://www.muggyweld.com/potmetal.html

Rob, check out this web site. They sell the aluminum scratch rod you are talking about only better. Their rod melts at half the melting point as the standard repair rod. 350 degrees as opposed to 700 degrees. We all know what happens to pot metal when you put a torch to it :( . Eastwood also sells the regular aluminum scratch rod but I only see it in the catalog not online. Hope this helps. Art :thumb:

Link to comment
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

  • Recently Browsing   0 members

    • No registered users viewing this page.
×
×
  • Create New...